挤压镁基混杂复合合金的纵向压痕蠕变研究
Extruded Mg based hybrid composite alloys studied by longitudinal impression creep
摘要:
研究了Saffil短纤维和SiC颗粒以不同组合增强的抗蠕变AE 42镁合金的纵向蠕变行为,在175-300 ℃的温度范围内,在60 - 140 MPa的应力水平下,使用压痕蠕变测试技术,含有随机纤维取向的平面平行于加载方向。在175 ℃下,正常的蠕变行为,即,应变速率随应变而降低,然后达到稳定状态,在所有使用的应力下观察到。在240 ℃下,观察到高达80 MPa的正常蠕变行为,在应力以上观察到应变速率随应变而增加,然后达到稳定状态并再次降低。在300 ℃时,在所有应力下均观察到反向蠕变行为.此模式对于所有复合材料保持相同。反向蠕变行为被发现与纤维断裂。发现所有复合材料的应力指数都很高。考虑门槛应力后,应力指数在3.9 ~ 7.0之间,表明粘滞滑移和位错攀移是主要的蠕变机制。由于在任何应力水平下正常或反向蠕变行为的数据不足,未计算表观活化能Qc。混合复合材料的抗蠕变性被认为是可比的,在所有的温度和应力水平的调查与20%的Saffil短纤维增强的复合材料。
英文摘要:
The creep behaviour of a creep-resistant AE42 magnesium alloy reinforced with Saffil short fibres and SiC particulates in various combinations has been examined in the longitudinal direction, i.e., the plane containing random fibre orientation was parallel to the loading direction, in the temperature range of 175-300 C at the stress levels ranging from 60 to 140 MPa using impression creep test technique. At 175 C, normal creep behaviour, i.e., strain rate decreasing with strain and then reaching a steady state, is observed at all the stresses employed. At 240 C, normal creep behaviour is observed up to 80 MPa and reverse creep behaviour, i.e., strain rate increasing with strain, then reaching a steady state and again decreasing, is observed above that stress. At 300 C, reverse creep behaviour is observed at all the stresses employed. This pattern remains the same for all the composites. The reverse creep behaviour is found to be associated with the fibre breakage. The stress exponent is found to be very high for all the composites. However, after taking the threshold stress into account, the stress exponent varies from 3.9 to 7.0, which suggests viscous glide and dislocation climb being the dominant creep mechanisms. The apparent activation energy Qc was not calculated due to insufficient data at any stress level either for normal or reverse creep behaviour. The creep resistance of the hybrid composites is found to be comparable to that of the composite reinforced with 20% Saffil short fibres at all the temperatures and stress levels investigated.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。