With infrared and terahertz ellipsometry we investigated the anisotropy of the infrared active phonon modes in SrTiO3 (110) single crystals in the tetragonal state below the so-called antiferrodistortive transition at T* = 105 K. In particular, we show that the anisotropy of the oscillator strength of the so-called R-mode, which becomes weakly infrared active below T*, is a valuable indicator for the orientation of the structural domains. Our results reveal that a mono-domain state with the tetragonal axis (c-axis) parallel to the [001] direction can be created by applying a moderate uniaxial stress of about 2.3 MPa along the [1-10] direction (with a mechanical clamp). The resulting, intrinsic splitting of the infrared-active phonon modes is reported.
Heteroepitaxial growth of tetragonal Mn$_{2.7-x}$Fe$_{x}$Ga$_{1.3}$ (0 $\leqslant$ x $\leqslant$ 1.2) Heusler films with perpendicular magnetic anisotropy
本文研究了不同Fe含量x(0 $\leqslant$ x $\leqslant$ 1.2)的Mn $_{2.7-x}$ Fe $_{x}$ Ga $_{1.3}$ Heusler薄膜的结构和磁性。采用磁控溅射法在MgO单晶衬底上异质外延生长薄膜。Mn $_{2.7-x}$ Fe $_{x}$ Ga $_{1.3}$薄膜的晶化厚度为35 nm,具有(001)择优取向的四方D 0 $_{22}$结构。通过改变Fe含量x,实现了磁性能的可调。Mn $_{2.7-x}$ Fe $_{x}$ Ga $_{1.3}$薄膜具有高的单轴各向异性,Ku $\geqslant$为1.4 MJ/m ~ 3,矫顽力为0.95 ~ 0.3 T,饱和磁化强度为290 ~ 570 kA/m。具有Mn $_{1.6}$ Fe $_{1.1}$ Ga $_{1.3}$组成的膜在室温下显示出1.47 MJ/m3的高Ku和37 kJ/m3的能量积${(BH)_{max}}$。这些发现表明Mn $_{2.7-x}$ Fe $_{x}$ Ga $_{1.3}$薄膜具有用于中程永磁体和自旋电子学应用的有希望的性质。
Concentration tuned tetragonal strain in alloys: application to magnetic anisotropy of FeNi$_{1-x}$Co$_x$
我们探索一个机会,诱导和控制材料中的四面体畸变。这个想法涉及从具有体心和面心对称性的母体化合物形成二元合金。这个概念的情况下说明的FeNi $_{1-x}$ Co $_x$磁性合金形成的替代掺杂的L1 $_0$ FeNi磁体与Co。使用电子结构计算,我们证明,在这个系统中的四重态应变可以控制的浓度,它达到最大值为$x=0.5$。这一发现,然后应用到创建一个大的磁晶各向异性(MAE)在FeNi $_{1-x}$ Co $_x$系统考虑的相互作用的四重态畸变与电子浓度和化学各向异性。特别是,我们确定了一个新的有序FeNi $_{0.5}$ Co $_{0.5}$系统,MAE大于L1 $_0$ FeNi磁体的4.5倍。
Magnetoelasticity - magnetic structure interrelation - tetragonal MnPt system study
IT4Innovations, VSB – Technical University of Ostrava(VSB-奥斯特拉发理工大学);Institute of Molecular Physics, Polish Academy of Sciences(波兰科学院分子物理研究所);Charles University, Faculty of Mathematics and Physics(查理大学数学物理学院);Institute of Low Temperature and Structure Research, Polish Academy of Sciences(波兰科学院低温结构研究所);Departamento de Física, Universidad de Oviedo(奥维耶多大学物理系)
Thermodynamically stable skyrmion lattice in tetragonal frustrated antiferromagnet with dipolar interaction
受最近关于GdRu $_2$ Si $_2$的实验结果的启发[Khanh,N.D.,Nakajima,T.,Yu,X.例如,\emph{Nat. Nanotechnol.} \textbf{15},444-449(2020)],其中观察到纳米正方形skyrmion晶格,我们提出了在外部磁场中具有偶极相互作用的中心对称四重阻挫反铁磁体的相图的高温部分的简单分析平均场描述。在倒易空间中,偶极力提供动量依赖的双轴各向异性。结果表明,在四元晶格中,对于$ab$平面上相互垂直的调制矢量,在布里渊区的大部分区域内,这种各向异性具有相互垂直的易磁化轴和共线的中间磁化轴,这导致双Q调制自旋结构的稳定化.后者原来是一个正方形的skyrmion晶格在其稳定区域的大部分与拓扑电荷$\pm 1$每个磁性单元格,这是由受抑的交换耦合,因此,纳米尺寸。当存在额外的单离子易轴各向异性时,易轴和中间轴可以互换,从而导致不同的相图。有人认为,后一种情况是相关的GdRu $_2$ Si $_2$。