SrTiO3表面的极性补偿(111)
Polar compensation at the surface of SrTiO3 (111)
摘要:
我们系统地研究了退火对SrTiO_3(111)极性表面的结构和组成的影响。Ti和Sr之间的相对表面浓度强烈地依赖于退火温度和氧处理。存在一个临界退火温度,在该温度下实现Ti与Sr的最大浓度比,同时仍保持(1 × 1)表面结构。我们证明,通过适当的处理,可以避免在很宽的温度范围内的表面重建。我们的研究结果提供了一个最佳的温度窗口外延薄膜生长。
英文摘要:
We have systematically investigated the annealing effect on the structure and composition of the polar surface of SrTiO3 (111), starting with an ex-situ chemical etch. The relative surface concentration between Ti and Sr strongly depends on both the annealing temperature and the oxygen processing. There is a critical annealing temperature at which the maximum concentration ratio of Ti to Sr is achieved, while still maintaining a (1 x 1) surface structure. We demonstrate that with proper processing it is possible to avoid surface reconstruction over a broad temperature range. Our results provide an optimal temperature window for epitaxial film growth.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。