收缩梯度诱导的硬化水泥石微裂纹
Contraction gradient induced microcracking in hardened cement paste
摘要:
混凝土表面和修补层的干燥开裂是一个常见的问题。这种类型的裂缝的主要原因是水分和干燥时在水泥浆基质中产生的收缩梯度。这种现象已被实验量化在无侧限硬化水泥浆样品使用荧光树脂浸渍技术。本文报道并解释了试样厚度和干燥方法对表面裂纹密度和裂纹穿透深度的影响。水分梯度的有限元模拟表明,在无侧限样品的干燥开裂膜系数的重要作用。取决于干燥方法,样品在干燥时保持无裂纹的临界厚度在2-5 mm的范围内。在较厚的样品中,观察到的裂纹间距加倍过程与理论预测一致。
英文摘要:
Drying induced cracking of concrete surfaces and repair layers is a common problem. A principal cause for this type of cracking is the moisture and resulting contraction gradient that develops in the cement paste matrix upon drying. This phenomenon has been experimentally quantified in unconfined hardened cement paste samples using a fluorescent resin impregnation technique. The effects of sample thickness and drying method on surface crack density and crack penetration depth are reported and explained. Finite element modelling of moisture gradients indicate the important role of the film coefficient in desiccation cracking of unconfined samples. The critical thickness for samples to remain crack-free upon drying was in the range of 2-5 mm depending on drying method. In thicker samples a crack spacing doubling process was observed that is in agreement with theoretical predictions.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。