挪威云杉的力学性能:早材和晚材的环内变异和一般行为直至破坏
Mechanical Properties of Norway Spruce: Intra-Ring Variation and Generic Behavior of Earlywood and Latewood until Failure
摘要:
早材和晚材交替的生长轮结构对挪威云杉的力学性能有很大的影响。在目前的研究中,在纵向和切向方向的拉伸试验进行了一系列的标本,代表一个生长环在不同的相对湿度。所有测试的力学参数,即弹性模量和极限拉伸应力,遵循密度分布在生长轮,最小值在早材和最大值在晚材。将样品在相对湿度50%、65%和95%的三个条件下进行调节。随着相对湿度的增加,力学参数的值被发现降低。然而,由于局部变异性较高,该降低不具有统计学显著性。在65%相对湿度下对早材和晚材试样进行的切线方向试验表明,早材和晚材的线弹性极限相似。当两种组织的强度相等时,早材的破坏应变明显更大。此外,早材的非线性应力/应变行为的部分显著更大。对极限拉伸强度的Weibull分析揭示了与组织无关的Weibull模量,这表明类似的缺陷分布。对于这两种情况,失效均发生在中间板层。
英文摘要:
The alternating earlywood and latewood growth ring structure has a strong influence on the mechanical performance of Norway spruce. In the current study, tensile tests in the longitudinal and tangential directions were performed on a series of specimens representing one growth ring at varying relative humidities. All tested mechanical parameters, namely modulus of elasticity and ultimate tensile stress, followed the density distribution in the growth ring, with the minimum values in earlywood and the maximum values in latewood. The samples were conditioned at three the relative humidities 50%, 65% and 95%. With increasing relative humidity, the values of the mechanical parameters were found to decrease. However, due to the high local variability, this decrease was not statistically significant. The test in the tangential direction on a set of earlywood and latewood specimens at 65% relative humidity revealed a similar limit of linear elasticity for both early- and latewood. Where the strength of both tissues was equal, the strain at failure was significantly greater for earlywood. Furthermore, the portion of the non-linear stress/strain behavior for earlywood was significantly greater. A Weibull analysis on the ultimate tensile strength revealed a tissue-independent Weibull modulus, which indicates similar defect distributions. For both, the failure occurred in the middle lamella.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。