磁性Bi $_{0.9}$ Gd $_{0.1}$ Fe $_{1-x}$ Ti $_x$ O $_3$纳米粒子的简单自顶向下制备
Simple top-down preparation of magnetic Bi$_{0.9}$Gd$_{0.1}$Fe$_{1-x}$Ti$_x$O$_3$ nanoparticles by ultrasonication of multiferroic bulk material
摘要:
我们提出了一种简单的技术,直接从块状多铁性钙钛矿粉末合成超细纳米粒子。起始材料是标称组成为Bi $_{0.9}$ Gd $_{0.1}$ Fe $_{1-x}$ Ti $_x$ O $_3$(x = 0.00-0.20)的陶瓷粒料,最初通过固态反应技术制备,然后研磨成微米级粉末并在超声浴中与异丙醇或水混合。用透射电子显微镜成像和电子衍射研究了粒度作为超声处理时间的函数,证实形成了大部分平均尺寸为11-13 nm的单晶纳米颗粒。在室温下,观察到Bi $_{0.9}$ Gd $_{0.1}$ Fe $_{1-x}$ Ti $_x$ O $_3$纳米颗粒与它们的本体对应物相比的磁行为的显著改善。这种超声技术可以被认为是一种简单而有前途的路线,以制备超细纳米粒子的功能应用。
英文摘要:
We present a simple technique to synthesize ultrafine nanoparticles directly from bulk multiferroic perovskite powder. The starting materials, which were ceramic pellets of the nominal compositions of Bi$_{0.9}$Gd$_{0.1}$Fe$_{1-x}$Ti$_x$O$_3$ (x = 0.00-0.20), were prepared initially by a solid state reaction technique, then ground into micrometer-sized powders and mixed with isopropanol or water in an ultrasonic bath. The particle size was studied as a function of sonication time with transmission electron microscopic imaging and electron diffraction that confirmed the formation of a large fraction of single-crystalline nanoparticles with a mean size of 11-13 nm. A significant improvement in the magnetic behavior of Bi$_{0.9}$Gd$_{0.1}$Fe$_{1-x}$Ti$_x$O$_3$ nanoparticles compared to their bulk counterparts was observed at room temperature. This sonication technique may be considered as a simple and promising route to prepare ultrafine nanoparticles for functional applications.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。