镍-碳纳米颗粒的尺寸依赖性phase diagrams
Size dependent phase diagrams of Nickel-Carbon nanoparticles
摘要:
镍-碳纳米颗粒的富碳相图,相关的催化和催化化学气相沉积合成的碳纳米管,计算系统的尺寸高达约3纳米(807镍原子)。原子间相互作用的紧束缚模型驱动用于定位固体、核/壳和液体稳定域的巨正则蒙特卡罗模拟,作为尺寸、温度和碳化学势或浓度的函数。熔融是有利的碳从纳米颗粒表面掺入,导致在一个强大的相对较低的共晶温度和相图拓扑结构不同于散装。在我们理解纳米管生长机制时,应考虑到这一点。
英文摘要:
The carbon rich phase diagrams of nickel-carbon nanoparticles, relevant to catalysis and catalytic chemical vapor deposition synthesis of carbon nanotubes, are calculated for system sizes up to about 3 nanometers (807 Ni atoms). A tight binding model for interatomic interactions drives the Grand Canonical Monte Carlo simulations used to locate solid, core/shell and liquid stability domains, as a function of size, temperature and carbon chemical potential or concentration. Melting is favored by carbon incorporation from the nanoparticle surface, resulting in a strong relative lowering of the eutectic temperature and a phase diagram topology different from the bulk one. This should be taken into account in our understanding of the nanotube growth mechanisms.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。