摘要:
采用原子力显微镜(AFM)和掠入射X射线衍射(GI-XRD)对旋涂低聚物的纳米形貌进行了表征。(LMW,Mn = 12 kg/mol,区域规整性RR = 84%)和高(HMW,Mn = 39 kg/mol,RR = 98%)分子量聚(3-己基硒醚)(P3 HS)膜和P3 HS与[6,6]-苯基-C61-丁酸甲酯(PCBM)的共混物膜,在250 ℃下热退火之前和之后。
英文摘要:
Atomic Force Microscopy (AFM) and Grazing Incidence X-Ray Diffraction (GI-XRD) are used to characterize the nanomorphology of spin-coated low (LMW, Mn = 12 kg/mol, regioregularity RR = 84%) and high (HMW, Mn = 39 kg/mol, RR = 98%) molecular weight poly(3-hexylselenophene) (P3HS) films and blend films of P3HS with [6,6]-phenyl-C61-butyric acid methyl ester (PCBM), before and after thermal annealing at 250 °C.