我们已经证明了OPV加速降解研究使用集中的阳光,其中的气氛,温度和光照强度是独立控制的。在集中的阳光下测试用于控制样品温度的各种方案表明,P3 HT:PCBM的加热是由吸收波长范围内的光子和多余光子能量的耗散引起的,而不一定是由IR光子吸收引起的。在集中太阳光照射下,太阳光斩波是一种有效的独立温度控制方法。报道了第一次使用施加于P3 HT:PCBM共混物的阳光浓度的加速降解测试。P3 HT:PCBM共混物暴露于在痕量氧气/湿度存在下的集中阳光下,显示出由P3 HT:PCBM共混物内的P3 HT主链的光氧化引起的降解,其显著地热加速,与先前的观察结果一致。然而,这可以以分钟和小时的时间尺度来证明,即,大大加快。将良好封装的P3 HT:PCBM膜暴露于集中的阳光下证明了高达3,600太阳 * 小时的稳定性,对应于约1.6年的操作时间。该结果是在300个太阳照射下仅12小时后获得的,证明了使用集中的太阳光进行加速稳定性试验的优点。因此,这些测试可以将极高的加速因子与对各种独立控制因素对降解机制的影响的深刻理解相结合。
英文摘要:
We have demonstrated OPV accelerated degradation studies using concentrated sunlight, where the atmosphere, temperature and illumination intensity were independently controlled. Testing various schemes for controlling the sample temperature under concentrated sunlight showed that heating of P3HT:PCBM was caused by photons at the absorbed wavelength range and dissipation of excess photon energy, and not necessarily by IR photon absorption. Sunlight chopping was found to be an effective method for independent temperature control under illumination by concentrated sunlight. The first accelerated degradation tests using sunlight concentration applied to P3HT:PCBM blends were reported. P3HT:PCBM blends exposed to concentrated sunlight in the presence of traces of oxygen/ humidity showed degradation induced by photo-oxidation of the P3HT backbone within the P3HT:PCBM blend, which is significantly thermally accelerated, in agreement with previous observations. However, this could be demonstrated in a time scale of minutes and hours, i.e., significantly accelerated. Exposure of well encapsulated P3HT:PCBM films to concentrated sunlight demonstrated stability up to 3,600 sun*hours, corresponding to about 1.6 years of operating time. This result was obtained at 300 suns exposure after merely 12 hours, demonstrating the advantage of using concentrated sunlight for accelerated stability tests. These tests can therefore combine extremely high acceleration factors with profound understanding of the effect of various, independently controlled factors on the degradation mechanisms.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。