arXiv 1408.4212physics.opticscond-mat.mtrl-sci
收藏

不同尺寸CsI:Na晶体的CL和PL特性

The CL and PL characteristic of different scale CsI:Na crystals

Jun-Peng Hu, Fang Liu, Xiao-Ping Ouyang

摘要:

研究了不同尺度CsI:Na晶体的光致发光(PL)和阴极发光(CL)激发的发光特性。将CsI:Na晶体加工成三种不同直径的样品,从微米级减小到纳米级。结果表明,纳米CsI:Na晶体的PL发射波长为420nm,CL发射波长为315nm和605nm。这种现象的产生与入射粒子的能量、密度以及CsI:Na晶体的直径有关。当晶体直径减小到纳米尺度时,表面缺陷相对增多,导致Na的相对发光降低。此外,我们还对CsI:Tl晶体进行了相同条件下的实验研究。结果表明,发光强度与晶体直径几乎无关。

英文摘要:

We investigate the luminescence characteristic of different scale CsI:Na crystals excited via photoluminescence(PL) and cathodoluminescence (CL). The CsI:Na crystals are processed to three samples with different diameter, decreasing from micro-scale to nano-scale. It is found that the nano-scale CsI:Na crystal emits 420nm luminescence by PL, while its emission band is at 315nm and 605nm by CL. The reason for this phenomenon relates to the energy and density of incident particles, and the diameter of CsI:Na crystal. When crystal diameter decreases to nano-scale, the number of surface defects relatively increases, leading to the Na-relative luminescence decreasing. In addition, we have also investigated the CsI:Tl crystal with the same experiment condition. The result indicates that the emission almost has nothing to do with the crystal diameter.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑