碱金属乙二胺插层超导体Ax(C2H8N2)yFe2-zSe2(A = Li,Na)(Tc = 45 K)的合成及退火后效应
Synthesis and post-annealing effects of alkaline-metal-ethylenediamine-intercalated superconductors Ax(C2H8N2)yFe2-zSe2 (A = Li, Na) with Tc = 45 K
摘要:
采用碱金属在乙二胺中的插层法,成功地合成了Tc = 45 K的新型铁基插层超导体Ax(C2 H8 N2)yFe 2-zSe 2(A = Li,Na)。Ax(C2 H8 N2)yFe 2-zSe 2(A = Li,Na)的c轴长度分别为20.74(7)nm和21.9(1)nm,比KxFe 2Se 2的长约50%,表明FeSe的Se-Se层间不仅有碱金属而且有乙二胺插层。Ax(C_2H_8N_2)_yFe_(2-z)Se_2(A = Li,Na)的高Tc可能是由于其c轴长度较大而可能具有的二维电子结构所致。通过在真空玻璃管中的后退火,已经发现Tc随着后退火温度的升高而降低,并且EDA从插层样品中的脱嵌发生在低于250 °C的低温下。
英文摘要:
New iron-based intercalation superconductors Ax(C2H8N2)yFe2-zSe2 (A = Li, Na) with Tc = 45 K have successfully been synthesized via intercalation of dissolved alkaline metal in ethylenediamine. The c-axis lengths of Ax(C2H8N2)yFe2-zSe2 (A = Li, Na) are 20.74(7) Å and 21.9(1) Å, respectively, and are about 50 % larger than that of KxFe2Se2, indicating that not only alkaline metal but also ethylenediamine is intercalated between the Se-Se layers of FeSe. It seems that the high-Tc of Ax(C2H8N2)yFe2-zSe2 (A = Li, Na) is caused by the possible two-dimensional electronic structure due to the large c-axis length. Through the post-annealing in an evacuated glass tube, it has been found that Tc decreases with increasing post-annealing temperature and that deintercalation of EDA from the as-intercalated sample takes place at low temperatures below 250 °C.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。