L-苏氨酸掺杂显著提高了KDP晶体的结晶完整性、二次谐波产生效率、光学透过率和laser损伤阈值
Remarkable enhancement in crystalline perfection, Second Harmonic Generation Efficiency, Optical Transparency and laser damage threshold in KDP crystals by L-threonine doping
摘要:
研究了L-苏氨酸(LT)掺杂对慢蒸发溶液法(SEST)生长的磷酸二氢钾(KDP)晶体的结晶完整性、二次谐波(SHG)效率、光学透过率和激光损伤阈值(LDT)的影响。研究了掺杂对晶体生长速率和形貌的影响。粉末X-射线衍射数据证实了KDP的晶体结构,并显示了由于不同的LT浓度与形态相关的衍射峰强度的系统变化。没有观察到额外的相形成,这通过傅里叶变换(FT)拉曼研究进一步证实。高分辨率的X射线衍射曲线表明,在低浓度下,晶体的完整性得到了很大程度的改善,在1摩尔%的掺杂最大的完善。在较高浓度(5至10摩尔%)下,由于在晶体基质的间隙位点处过量掺入掺杂剂,其略微降低。随着掺杂浓度的增加,LDT显著增加,而SHG效率在1 mol%时最大,与晶体相关。与纯KDP相比,掺杂晶体的光学透明度已增加,在1摩尔%掺杂时具有最大值。
英文摘要:
Effect of L-threonine (LT) doping on crystalline perfection, second harmonic generation (SHG) efficiency, optical transparency and laser damage threshold (LDT) in potassium dihydrogen phosphate (KDP) crystals grown by slow evaporation solution technique (SEST) has been investigated. The influence of doping on growth rate and morphology of the grown crystals has also been studied. Powder X-ray diffraction data confirms the crystal structure of KDP and shows a systematic variation in intensity of diffraction peaks in correlation with morphology due to varying LT concentration. No extra phase formation was observed which is further confirmed by Fourier Transform (FT) Raman studies. High-resolution X-ray diffraction curves indicate that crystalline perfection has been improved to a great extent at low concentrations with a maximum perfection at 1 mol% doping. At higher concentrations (5 to 10 mol%), it is slightly reduced due to excess incorporation of dopants at the interstitial sites of the crystalline matrix. LDT has been increased considerably with increase in doping concentration, whereas SHG efficiency was found to be maximum at 1 mol% in correlation with crystalline. The optical transparency for doped crystals has been increased as compared to that of pure KDP with a maximum value at 1 mol% doping.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。