氧化铝和氧化锆增韧氧化铝(ZTA)髋关节假体在冲击装置中微分离条件下的降解试验

Degradation of alumina and zirconia toughened alumina (ZTA) hip prostheses tested under microseparation conditions in a shock device

Juliana Uribe, Jean Geringer, Laurent Gremillard, Bruno Reynard

摘要:

本文考虑了氧化铝和氧化锆增韧氧化铝与氧化铝用于髋关节植入物的降解。材料被假定为在潮湿条件下经受冲击的承载表面。载荷是力的峰值;以2 Hz在15 ms内施加9 kN,持续800,000次循环。ZTA的体积磨损和粗糙度低于氧化铝。长时间的ZTA老化似乎对粗糙度没有直接影响。老化增加了ZTA的磨损体积,并且发现与氧化铝相比具有更高的耐磨性。

英文摘要:

This paper considers the degradation of alumina and zirconia toughened alumina vs. alumina for hip implants. The materials are as assumed to be load bearing surfaces subjected to shocks in wet conditions. The load is a peak of force; 9 kN was applied over 15 ms at 2 Hz for 800,000 cycles. The volumetric wear and roughness are lower for ZTA than for alumina. The long ZTA ageing did not seem to have a direct influence on the roughness. The ageing increased the wear volumes of ZTA and it was found to have a higher wear resistance compared to alumina.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑