含ScCO2自掺杂纳米聚苯胺的水性环氧涂料的防护性能

Protective Performance of Water-Based Epoxy Coating Containing ScCO2 Synthesized Self-Doped Nanopolyaniline

M. R. Bagherzadeh, T. Mousavinejad, E. Akbarinezhad, A. Ghanbarzadeh

摘要:

采用超临界二氧化碳(ScCO 2)介质合成了自掺杂纳米聚苯胺(SPAni),并将其添加到水性环氧涂料中,以改善涂料的耐腐蚀性能。以ScCO 2合成的自掺杂纳米聚苯胺(SPAni)为原料,采用水性聚酰胺-胺固化剂对其进行改性,得到了水性SPAni复合材料(Sc-WB)。将Sc-WB与环氧树脂按化学计量比混合,得到水性聚苯胺环氧涂料(SP-WBE)。利用扫描电子显微镜(SEM)研究了SP-WBE在腐蚀介质中氧化层的形成和附着性能。利用透射电子显微镜(TEM)观察了纳米聚苯胺在最终干燥膜中的分布和粒径。采用ASTM B-117盐雾标准试验、电化学阻抗谱(EIS)和附着力试验研究了水性环氧涂层试样(空白涂层试样)和SP-WBE涂层试样的耐腐蚀性能。结果表明,在ScCO 2气氛下合成的自掺杂聚苯胺可提高水性环氧涂料的防护性能。在3.5Wt%NaCl水溶液中浸泡1800小时后,含纳米聚苯胺的涂层和空白样品的电阻分别为1.8778E+7 Ω·cm ~ 2和2.512E+5 Ω·cm ~ 2。

英文摘要:

In this research, corrosion properties of water-based epoxy coating is improved by adding self-doped nano polyaniline (SPAni) synthesized using supercritical carbon dioxide (ScCO2) medium. The modified ScCO2-synthesized self-doped nano polyaniline (SPAni) using water-based polyamidoamine hardener results formation of the water-based SPAni composite (Sc-WB). To obtain the water-based polyaniline epoxy coating (SP-WBE), the Sc-WB was mixed with epoxy resin in stoichiometric ratio. The formation of oxide layers and adhesion properties of SP-WBE at corrosive medium was evaluated using scanning electron microscopy (SEM) studies. The transmission electron microscopy (TEM) was used to observe the distribution and particles size of nanopolyaniline in the final dried film. The anti-corrosion performance of water-based epoxy coated sample (blank coated sample) and SP-WBE coated sample was studied using salt spray standard test according to ASTM B-117, electrochemical impedance spectroscopy (EIS) and adhesion tests. The results indicate protective performance of water-based epoxy coating is improved by adding self-doped polyaniline synthesized at ScCO2 situation. The electrical resistance of the coatings containing nanopolyaniline and the blank sample was 1.8778E+7 Ω.cm2 and 2.512E+5 Ω.cm2 after 1800 hours of immersion in 3.5 Wt% NaCl aqua corrosive solutions.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑