掺铬石英光纤:纤芯成分对Cr氧化态和晶场的影响

Chromium-doped silica optical fibres : influence of the core composition on the Cr oxidation states and crystal field

Valérie Felice, Bernard Dussardier, Julian K. Jones, Gérard Monnom, Daniel B. Ostrowsky

摘要:

我们用改进的化学气相沉积法制备了掺铬的硅基预制件和光纤,并研究了掺杂区的化学组成对样品的铬氧化态和光谱性质的影响。最初作为Cr 3+引入的铬在制造过程中部分或全部氧化,并且在预制件和纤维的芯中作为八面体配位的Cr 3+和/或作为扭曲四面体配位(Cs)的Cr 4+稳定。二氧化硅中的小浓度(~1-2摩尔%)共掺杂剂,例如锗或铝,足以促进特定的氧化态。特别地,1摩尔%的铝将所有存在的铬稳定为Cr 4+。导出了Cr ~(3+)和Cr ~(4+)的配位场参数Dq、B和Dq/B。结果表明,样品中的铬离子处于中低配位场,Dq和Dq/B随铝含量的增加而减小。Cr 3+的吸收截面与玻璃和晶体中报道的相似,而Cr 4+的吸收值低于参考激光材料。

英文摘要:

We have made chromium-doped, silica-based preforms and optical fibres by Modified Chemical Vapour Deposition and have studied the influence of the chemical composition of the doped region on the Cr-oxidation states and the spectroscopic properties of the samples. Chromium, introduced initially as Cr3+, is partially or totally oxidized during the fabrication process, and is stabilized in the core of the preforms and fibres as Cr3+ in octahedral coordination, and/or as Cr4+ in distorded tetrahedral coordination (Cs). Small concentrations (~1-2 mol%) of codopants in silica, such as germanium or aluminium, suffice to promote a particular oxidation state. Particularly, 1 mol % of aluminium stabilizes all present chromium into Cr4+. The ligand field parameters, Dq, B and Dq/B, for Cr3+ and Cr4+ are derived. It is shown that the chromium ions in our samples are in low to intermediate ligand field and that Dq and Dq/B decrease when the aluminium content increases. The absorption cross sections of Cr3+ are similar to that reported in glasses and crystals, whereas Cr4+ has lower values than reference laser materials.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑