摘要:
本文报道了Bi-Sr-Ca-Cu-O(BSCCO)晶须状高温超导体的光电导和退火实验。单相Bi 2Sr 2CaCu 2 O 8 +δ(Bi-2212)样品和混合相Bi 2Sr 2Ca 2Cu 3 O 10 +x(Bi-2223)/Bi-2212的晶体都在90°C下在空气中经过几个小时的退火处理,最大总退火时间为47 h。在每个步骤中,样品通过在黑暗中和在UV-VIS卤素弧光灯的照射下的电阻与温度(R vs T)和在固定温度下的电阻与时间(R vs t)测量来表征。从这两种技术的结果的仔细比较已经表明,虽然对于单相样品没有效果被记录,对于混合相样品,随着退火时间的增加而增加的电导率的增强由标称温度T = 100 K下的光诱导,即在两相的临界温度之间的中间温度下。基于Kudinov方案的简单伪1D模型[Kudinov等人,Phys.Rev.B47,9017-28,(1993)]已经被开发来解释所观察到的效应,其基于嵌入Bi-2212基质中的Bi-2223细丝的存在以及在它们的界面处的电子活性缺陷的存在。该模型再现了相当好的光电导实验结果,并表明,随着退火时间的增加,Bi-2223细丝的长度减小,缺陷的数量增加。
英文摘要:
We report on combined photoconductivity and annealing experiments in whisker-like crystals of the Bi-Sr-Ca-Cu-O (BSCCO) high-Tc superconductor. Both single-phase Bi2Sr2CaCu2O8+δ(Bi-2212) samples and crystals of the mixed phases Bi2Sr2Ca2Cu3O10+x (Bi-2223)/Bi-2212 have been subjected to annealing treatments at 90°C in air in a few hours steps, up to a maximum total annealing time of 47 h. At every step, samples have been characterized by means of electrical resistance vs temperature (R vs T) and resistance vs time at fixed temperature (R vs t) measurements, both in the dark and under illumination with a UV-VIS halogen arc lamp. A careful comparison of the results from the two techniques has shown that, while for single-phase samples no effect is recorded, for mixed-phase samples an enhancement in the conductivity that increases with increasing the annealing time is induced by the light at the nominal temperature T = 100 K, i.e. at an intermediate temperature between the critical temperatures of the two phases. A simple pseudo-1D model based on the Kudinov's scheme [Kudinov et al., Phys. Rev. B 47, 9017-28, (1993)] has been developed to account for the observed effects, which is based on the existence of Bi-2223 filaments embedded in the Bi-2212 matrix and on the presence of electronically active defects at their interfaces. This model reproduces fairly well the photoconductive experimental results and shows that the length of the Bi-2223 filaments decreases and the number of defects increases with increasing the annealing time.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。