碘化铯薄膜结构的X射线衍射和透射电镜研究
Structural characterization of as-deposited cesium iodide films studied by X-ray diffraction and transmission electron microscopy techniques
摘要:
采用热蒸发技术制备了不同厚度的碘化铯(CsI)薄膜。利用X射线衍射(XRD)分析和透射电子显微镜(TEM)计数对薄膜的晶粒尺寸和晶粒尺寸进行了比较。这两种方法提供的微晶尺寸和晶粒尺寸之间的偏差较小的情况下,薄的CsI膜的4 nm,但有比较大的差异的情况下,较厚的CsI膜(20 nm,100 nm和500 nm)。这表明位错的排列方式使相邻共格区之间的取向差很小。从XRD获得的尺寸对应于两个单独的区域,而在TEM显微照片中,这两个区域似乎对应于一个区域,特别是在较厚膜的情况下。在均匀变形模型(UDM)、均匀变形应力模型(UDSM)和均匀变形能量密度模型(UDEDM)的假设下,采用修正的Williamson-Hall(W-H)分析方法,对$2θ= 20^{0}-80^{0}$范围内的CsI厚膜的主要XRD峰的应变、应力和变形能量密度等物理参数也进行了精确估算.
英文摘要:
In the present work, cesium iodide (CsI) thin films of different thickness have been prepared by thermal evaporation technique. The crystallite size and grain size of these films are compared by using X-ray diffraction (XRD) profile analysis as well as by transmission electron microscopy (TEM) counting, respectively. These two methods provide less deviation between crystallite size and grain size in the case of thin CsI films of 4 nm, but there is comparatively large difference in case of thicker CsI films (20 nm, 100 nm and 500 nm). It indicates that dislocations are arranged in a configuration which causes small orientational difference between two adjacent coherent regions. The size obtained from XRD corresponds to two separate regions, whereas in the TEM micrograph the two regions may seem to correspond one region particularly in case of thicker films. Other physical parameters such as strain, stress and deformation energy density are also estimated precisely for the prominent XRD peaks of thicker CsI films in the range $2θ= 20^{0}-80^{0}$ by using a modified Williamson-Hall (W-H) analysis assuming uniform deformation model (UDM), uniform deformation stress model (UDSM) and uniform deformation energy density model (UDEDM).
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。