白光干涉法在离子溅射表面定量表征中的应用

White Light Interferometry for Quantitative Surface Characterization in Ion Sputtering Experiments

S. V. Baryshev, A. V. Zinovev, C. E. Tripa, R. A. Erck, I. V. Veryovkin

摘要:

白光干涉技术可以获得毫米级的表面形貌信息,横向分辨率可达1 μm,深度分辨率可达1 nm。通过对样品表面进行真正的三维成像,WLI技术能够准确地定量表征表面特征的几何形状,并通过避免扫描电子显微镜和原子力显微镜的一些缺点而与它们进行比较。本文报道了用WLI成像技术表征离子溅射实验产物的结果。用几个图,WLI方法的几个示例应用被示出当用于(i)溅射产率测量和时间-深度转换,(ii)优化离子束电流密度分布、溅射坑的形状和多离子束叠加,以及(iii)用离子处理的表面的定量表征。特别是,溅射深度剖析实验的25镁,44钙和53铬离子注入Si(注入能量为1千电子伏每核子),由WLI方法确定的测量深度剖面曲线的深度校准似乎是自相一致的TRIM模拟这样的射弹矩阵系统。此外,利用气体团簇离子束对Genesis太阳风Si集热器表面进行处理,结果表明WLI方法具有很高的深度分辨率:处理后的表面去除了12.5 nm的薄层,而处理区与未处理区之间的过渡长度为150 μm。

英文摘要:

White light interferometry (WLI) can be used to obtain surface morphology information on dimensional scale of millimeters with lateral resolution as good as ~1 μm and depth resolution down to 1 nm. By performing true three-dimensional imaging of sample surfaces, the WLI technique enables accurate quantitative characterization of the geometry of surface features and compares favorably to scanning electron and atomic force microscopies by avoiding some of their drawbacks. In this paper, results of using the WLI imaging technique to characterize the products of ion sputtering experiments are reported. With a few figures, several example applications of the WLI method are illustrated when used for (i) sputtering yield measurements and time-to-depth conversion, (ii) optimizing ion beam current density profiles, the shapes of sputtered craters, and multiple ion beam superposition and (iii) quantitative characterization of surfaces processed with ions. In particular, for sputter depth profiling experiments of 25Mg, 44Ca and 53Cr ion implants in Si (implantation energy of 1 keV per nucleon), the depth calibration of the measured depth profile curves determined by the WLI method appeared to be self-consistent with TRIM simulations for such projectile-matrix systems. In addition, high depth resolution of the WLI method is demonstrated for a case of a Genesis solar wind Si collector surface processed by gas cluster ion beam: a 12.5 nm layer was removed from the processed surface, while the transition length between the processed and untreated areas was 150 μm.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑