通过配分、偏析和动态凝固的纳米级奥氏体逆转:韧性2GPa Fe-Cr-C钢的实例
Nanoscale austenite reversion through partitioning, segregation, and kinetic freezing: Example of a ductile 2 GPa Fe-Cr-C steel
摘要:
Fe-13.6Cr-0.44C钢回火过程中的奥氏体回复(wt. %)马氏体导致具有优异延展性的高强度铁素体不锈钢。奥氏体逆转机制与马氏体和残余奥氏体之间的界面处的低温分配期间碳的动力学冻结以及马氏体-马氏体晶界处的碳偏析相耦合。奥氏体回复的优点是其可扩展性,即,改变回火时间和温度可调整所需的强度-延展性曲线(例如,在400 ° C下回火1分钟产生2 GPa的极限拉伸强度(UTS)和14%的伸长率,而在400 ° C下回火30分钟产生约1.75 GPa的UTS和23%的伸长率)。通过XRD、EBSD、TEM和原子探针断层扫描(APT)对奥氏体逆转过程、碳化物沉淀和碳偏析进行了表征,以开发控制材料强度和延展性的结构-性能关系。
英文摘要:
Austenite reversion during tempering of a Fe-13.6Cr-0.44C (wt.%) martensite results in an ultrahigh strength ferritic stainless steel with excellent ductility. The austenite reversion mechanism is coupled to the kinetic freezing of carbon during low-temperature partitioning at the interfaces between martensite and retained austenite and to carbon segregation at martensite-martensite grain boundaries. An advantage of austenite reversion is its scalability, i.e., changing tempering time and temperature tailors the desired strength-ductility profiles (e.g. tempering at 400°C for 1 min. produces a 2 GPa ultimate tensile strength (UTS) and 14% elongation while 30 min. at 400°C results in a UTS of ~ 1.75 GPa with an elongation of 23%). The austenite reversion process, carbide precipitation, and carbon segregation have been characterized by XRD, EBSD, TEM, and atom probe tomography (APT) in order to develop the structure-property relationships that control the material's strength and ductility.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。