残余氧存在下硅化铒的生长
Erbium Silicide Growth in the Presence of Residual Oxygen
摘要:
研究了高真空蒸发和快速热退火非原位生长的Ti/Er/n-Si(100)叠层的化学变化。重点研究了退火温度对Er-Si固态反应和氧向Ti中渗透及其与Er相互作用的影响。为此,分析了三种类型的试样:沉积态、在300°C下退火和在600°C下退火。结果发现,残留的氧气进入退火气氛的存在下,导致在一个实质性的氧化的Er膜表面,无论退火温度。然而,Er膜与Si块体紧密接触的部分形成了总是不含氧的硅化物(在300°C下为非晶,在600°C下为结晶),如通过X射线光电子能谱学深度分布和在600°C下0.3 eV的肖特基势垒高度提取所证明的。这证明,即使Er对氧污染高度敏感,在n-Si上形成低肖特基势垒Er硅化物接触也是相当稳健的。最后,在工艺优化后,生产剥离无氧硅化铒。
英文摘要:
The chemical changes of Ti/Er/n-Si(100) stacks evaporated in high vacuum and grown ex situ by rapid thermal annealing were scrutinized. The emphasis was laid on the evolution with the annealing temperature of (i) the Er-Si solid-state reaction and (ii) the penetration of oxygen into Ti and its subsequent interaction with Er. For that sake, three categories of specimens were analyzed: as-deposited, annealed at 300°C, and annealed at 600°C. It was found that the presence of residual oxygen into the annealing atmosphere resulted in a substantial oxidation of the Er film surface, irrespective of the annealing temperature. However, the part of the Er film in intimate contact with the Si bulk formed a silicide (amorphous at 300°C and crystalline at 600°C) invariably free of oxygen, as testified by x-ray photoelectron spectroscopy depth profiling and Schottky barrier height extraction of 0.3 eV at 600°C. This proves that, even if Er is highly sensitive to oxygen contamination, the formation of low Schottky barrier Er silicide contacts on n-Si is quite robust. Finally, the production of stripped oxygen-free Er silicide was demonstrated after process optimization.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。