用于低温space telescopes的混合C/SiC复合材料的高精度CTE测量

High-precision CTE measurement of hybrid C/SiC composite for cryogenic space telescopes

K. Enya, N. Yamada, T. Imai, Y. Tange, H. Kaneda, H. Katayama, M. Kotani, K. Maruyama, M. Naitoh, T. Nakagawa, T. Onaka, M. Suganuma, T. Ozaki, M. Kume, M. R. Krodel

摘要:

本文介绍了高精度测量的“混合”碳纤维增强碳化硅复合材料,HB-Cesic \textregistered -ECM的商标,在\sim 310- 10 K的温度范围内的热膨胀。虽然C/SiC复合材料已被认为是有前途的反射镜和其他结构的航天低温望远镜,各向异性的热膨胀一直是这种材料的一个潜在的缺点。HB-Cesic \textregistered是一种新开发的复合材料,使用不同类型的短切碳纤维的混合物,其中开发的重要目的之一是减少各向异性。测量结果表明,各向异性大大降低到4%作为杂交的结果。获得的热膨胀数据作为温度的函数,分别使用八阶多项式的水平(XY-)和垂直(Z-)方向的制造过程。由XY和Z方向的数据得出的293- 10 K范围内的平均CTE及其分散度(1σ)分别为0.805 $\pm$ 0.003 \times 10 $^{-6}$ K $^{-1}$和0.837 \pm 0.001 \times 10 $^{-6}$ K $^{-1}$。本测量的绝对精度和重现性分别优于0.01 \times 10 $^{-6}$ K $^{-1}$和0.001 \times(10)^{-6} K^{-1}。热膨胀的残余各向异性与我们先前关于碳纤维的推测一致,其中残余各向异性倾向于主要位于水平面中。

英文摘要:

This paper presents highly precise measurements of thermal expansion of a "hybrid" carbon-fiber reinforced silicon carbide composite, HB-Cesic\textregistered - a trademark of ECM, in the temperature region of \sim310-10K. Whilst C/SiC composites have been considered to be promising for the mirrors and other structures of space-borne cryogenic telescopes, the anisotropic thermal expansion has been a potential disadvantage of this material. HB-Cesic\textregistered is a newly developed composite using a mixture of different types of chopped, short carbon-fiber, in which one of the important aims of the development was to reduce the anisotropy. The measurements indicate that the anisotropy was much reduced down to 4% as a result of hybridization. The thermal expansion data obtained are presented as functions of temperature using eighth-order polynomials separately for the horizontal (XY-) and vertical (Z-) directions of the fabrication process. The average CTEs and their dispersion (1σ) in the range 293-10K derived from the data for the XY- and Z-directions were 0.805$\pm$0.003\times10$^{-6}$ K$^{-1}$ and 0.837\pm0.001\times10$^{-6}$ K$^{-1}$, respectively. The absolute accuracy and the reproducibility of the present measurements are suggested to be better than 0.01\times10$^{-6}$ K$^{-1}$ and 0.001\times(10)^{-6} K^{-1}, respectively. The residual anisotropy of the thermal expansion was consistent with our previous speculation regarding carbon-fiber, in which the residual anisotropy tended to lie mainly in the horizontal plane.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑