粉末套管原位加工MgB2线材的拉伸诱导织构和拉伸性能随热处理时间的演变
Drawing induced texture and the evolution of superconductive properties with heat treatment time in powder-in-tube in-situ processed MgB2 strands
摘要:
将单芯粉末管MgB 2股线在600 ℃和700 ℃下冷拉和热处理长达71小时,并检查结构-性能关系。拉伸引起的Mg颗粒的伸长导致,HT后,由细长的多晶MgB 2纤维分离的细长孔组成的纹理化的宏观结构。超导Tc、Jc和Fp与宏观结构和晶粒尺寸有关。在600 ℃和700 ℃下,晶粒尺寸均随热处理时间的延长而增大。Jc和Fp随晶粒尺寸单调下降,但不是线性下降。总体而言,观察到在700 ℃下,MgB 2反应在短至30分钟后或多或少完成;在600 ℃下,直到71小时才发生完全反应完成。进入HT。在垂直施加场中测量传输Jct(B),并且分别在垂直和平行(轴向)施加场中测量磁临界电流密度Jcm \bot(B)和Jcm Tcm(B)。特别值得注意的是,在远低于Jct(B)的不可逆性场的场中,Jcm \bot(B)过早下降。这种效应归因于纤维宏观结构及其伴随的各向异性连接。磁场沿股线轴线方向的磁场测量得出一个临界密度Jcm \bot(B),即横向于股线轴线流动的电流密度,它小于Jct(B),且下降得比Jct(B)快。在传统的磁测量中,支持磁化的回路电流受到Jct(B)和Jcm(B)中较低者的限制。在当前情况下,后者导致测量的Jcm(B)与Jct(B)相比随着场的增加而过早下降。这一结果得到了Jcm τ(B)和Jct(B)数据的Kramer图的支持,该图导致横向电流的不可逆性场比通常的运输测量纵向场Birr,t小得多。
英文摘要:
Monocore powder-in-tube MgB2 strands were cold-drawn and heat-treated at 600C and 700C for times of up to 71 hours and structure-property relationships examined. Drawing-induced elongation of the Mg particles led, after HT, to a textured macrostructure consisting of elongated polycrystalline MgB2 fibers separated by elongated pores. The superconducting Tc, Jc and Fp were correlated with the macrostructure and grain size. Grain size increased with HT time at both 600C and 700C. Jc and hence Fp decreased monotonically but not linearly with grain size. Overall, it was observed that at 700C, the MgB2 reaction was more or less complete after as little as 30 min; at 600C, full reaction completion did not occur until 71 h. into the HT. Transport, Jct(B) was measured in a perpendicular applied field, and the magnetic critical current densities, Jcm\bot(B) and Jcmϕ(B), were measured in perpendicular and parallel (axial) applied fields, respectively. Particularly noticeable was the premature dropoff of Jcm\bot(B) at fields well below the irreversibility field of Jct(B). This effect is attributed to the fibrous macrostructure and its accompanying anisotropic connectivity. Magnetic measurements with the field directed along the strand axis yielded a critical density, Jcm\bot(B), for current flowing transversely to the strand axis that was less than and dropped off more rapidly than Jct(B). In the conventional magnetic measurement, the loop currents that support the magnetization are restricted by the lower of Jct(B) and Jcmϕ (B). In the present case the latter, leading to the premature dropoff of the measured Jcm(B) compared to Jct(B) with increasing field. This result is supported by Kramer plots of the Jcmϕ (B) and Jct(B) data which lead to an irreversibility field for transverse current that is very much less than the usual transport-measured longitudinal one, Birr,t.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。