与Pb基磁电层压板(MEL)相比,我们发现在BaTiO 3和NiFe 2 O 4层压板(层数n = 5-25)中,由于磁矩沿NiFe 2 O 4平面的优先排列,纵向磁电(ME)电压系数α E33变得比横向大得多。此外,在将每个层的厚度减小到15 μ m时,我们实现了高达18 mV/(cm Oe)的增强的Alpha E33和与n成比例的ME灵敏度的系统性增加,以实现无铅MEL中的最大值(400*10^-6V/Oe),从而为在大规模生产的环境友好层压板中定制ME耦合提供了途径。
英文摘要:
In contrast to the Pb-based magnetoelectric laminates (MELs), we find in the BaTiO3 and NiFe2O4 laminates (number of layers n = 5-25) that the longitudinal magnetoelectric (ME) voltage coefficient Alpha E33 becomes much larger than the transverse one due to preferential alignment of magnetic moments along the NiFe2O4 plane. Moreover, upon decreasing each layer thickness down to 15 um, we realize enhanced Alpha E33 up to 18 mV/ (cm Oe) and systematic increase of the ME sensitivity in proportion to n to achieve the largest in the Pb-free MELs (400*10^-6V/Oe), thereby providing pathways for tailoring ME coupling in mass-produced, environment friendly laminates.
Magnetoelectric effects of nanoparticulate Pb(Zr0.52Ti0.48)O3-NiFe2O4 composite films
我们制备了Pb(Zr0.52Ti0.48)O3-NiFe 2 O 4复合薄膜,该复合薄膜由NiFe 2 O 4纳米颗粒随机分散在Pb(Zr0.52Ti0.48)O3基体中组成。结构分析表明,NiFe 2 O 4纳米粒子的晶轴与铁电基体的晶轴对齐。该复合材料具有良好的铁电和磁性。我们测量的磁电电压系数的横向和纵向分量,这支持的假设,磁电效应来自磁致伸缩NiFe 2 O 4和压电Pb(Zr0.52Ti0.48)O3颗粒之间的直接应力耦合。
Magnetic field driven enhanced ferroelectric switching in self-grown ferroelectric-ferromagnetic composite in the BiFeO3-BaTiO3 multiferroic alloy system
多年来,人们试图弥补多铁性BiFeO 3体相态的固有弱点,如高漏电流和铁磁相关性的缺乏,并通过与其他钙钛矿形成固溶体来利用其磁电势。近几年的研究表明,BiFeO_3与BaTiO_3的合金化,无论有无添加剂,都可以诱导铁电和铁磁开关。虽然从技术应用的角度来看,这两种铁性序的共存是令人鼓舞的,但该系统中铁磁性的起源仍然难以捉摸。在这里,我们合成了这样的组合物,并进行了详细的结构分析,采用磁性分离的粉末颗粒。我们发现,铁磁性的起源在于自发沉淀的一个小的(~ 1wt%)钡六角铁氧体(BaFe 9 O 19)相,通常未检测到在常规的X射线衍射研究从整个标本的粉末取样。我们还表明,尽管微不足道的分数的亚铁磁相,这种自生长的复合材料表现出显着增强的铁电开关在外部磁场的存在下。我们得到了一个直流磁电耦合~ 9 × 10-8 s/m,这是一个值,这是已报道的层状铁电/铁磁层压板和双层薄膜铁电-铁磁hetrostructures。我们的研究表明,合理的大磁电耦合是可实现的,在简单的0-3铁电-铁磁块状复合材料提供的合成策略的开发,诱导自发沉淀的铁磁相在小体积分数,以确保良好的绝缘行为的复合材料,从而开发。