arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1106.4071cond-mat.str-el
收藏

商用超导量子干涉装置磁强计中用于磁性测量的微型陶瓷砧高压池

Miniature ceramic-anvil high-pressure cell for magnetic measurements in a commercial superconducting quantum interference device magnetometer

Naoyuki Tateiwa, Yoshinori Haga, Zachary Fisk, Yoshichika Onuki

摘要:

研制了一种用于商用超导量子干涉仪(SQUID)磁场测量的微型对顶高压室。采用复合陶瓷材料制成的非磁性砧座与Cu-Be垫片一起产生高压。我们检查了不同底脚尺寸(1.8、1.6、1.4、1.2、1.0、0.8和0.6 mm)的砧座。低温下产生的压力由铅(Pb)超导转变的压力依赖性决定。最大压力$P_{max}$取决于钉砧的底脚尺寸:1.8 mm和0.6 mm底脚钉砧的$P_{max}$值分别为2.4和7.6 GPa。我们发现,复合陶瓷顶锤有潜力产生高于5 GPa的高压。对于压头单元,Cu-Be垫圈的背景磁化强度通常比Ni-Cr-Al垫圈小两个数量级。本发明的电池不仅可以用于具有大磁化强度的铁磁和超导材料,而且可以用于具有较小磁化强度的反铁磁化合物。本发明的压力单元的生产成本约为金刚石砧单元的十分之一。由于复合陶瓷砧的强断裂韧性(6.5 MPa ${\cdot}$ m $^{1/2}$),在本压力单元中砧对准机构不是必需的。对于不熟悉高压技术的研究人员来说,简化的压力传感器易于使用。本文报道了超导MgB $_2$和反铁磁体CePd $_5$ Al $_2$的磁化强度的代表性结果。

英文摘要:

A miniature opposed-anvil high-pressure cell has been developed for magnetic measurement in a commercial superconducting quantum interference device (SQUID) magnetometer. Non-magnetic anvils made of composite ceramic material were used to generate high-pressure with a Cu-Be gasket. We have examined anvils with different culet sizes (1.8, 1.6, 1.4, 1.2, 1.0, 0.8 and 0.6 mm). The pressure generated at low temperature was determined by the pressure dependence of the superconducting transition of lead (Pb). The maximum pressure $P_{max}$ depends on the culet size of the anvil: the values of $P_{max}$ are 2.4 and 7.6 GPa for 1.8 and 0.6 mm culet anvils, respectively. We revealed that the composite ceramic anvil has potential to generate high pressure above 5 GPa. The background magnetization of the Cu-Be gasket is generally two orders of magnitude smaller than the Ni-Cr-Al gasket for the indenter cell. The present cell can be used not only with ferromagnetic and superconducting materials with large magnetization but also with antiferromagnetic compounds with smaller magnetization. The production cost of the present pressure cell is about one tenth of that of a diamond anvil cell. The anvil alignment mechanism is not necessary in the present pressure cell because of the strong fracture toughness (6.5 MPa${\cdot}$m$^{1/2}$) of the composite ceramic anvil. The simplified pressure cell is easy-to-use for researchers who are not familiar with high pressure technology. Representative results on the magnetization of superconducting MgB$_2$ and antiferromagnet CePd$_5$Al$_2$ are reported.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑