纳米晶铜铁氧体薄膜磁性能的温度依赖性
Temperature dependence of Magnetic properties in Nanocrystalline copper ferrite thin films
摘要:
采用射频溅射法在50 W的射频功率下制备了铜铁氧体薄膜。在空气中在$800^{\circ}$ C下对所沉积的膜进行退火,然后缓慢冷却。使用SQUID磁强计研究了沉积态(AD)和慢冷态(SC)薄膜。在5 ~ 300 K的温度范围内记录了M-H曲线。然后将从MH曲线获得的结晶度相对于温度(T)作图。即使在7 T的最高磁场下,薄膜中的磁化强度也不饱和。使用Chikazumi表达式M(H)= Q*(1- a /Hn)(n=1/2)的H1/2项来拟合M-H曲线的高场部分。观察到H_(1/2)项系数a随温度T的变化。已尝试将此与退火膜的情况下的结晶度(Hc)相关联。
英文摘要:
The copper ferrite thin films have been deposited by RF sputtering at a 50W rf power. The As-deposited films are annealed in air at $800^{\circ}$C and then slow cooled. The As-deposited (AD) as well as slow cooled (SC) films are studied using a SQUID Magnetometer. The M Vs H curves have been recorded at various temperatures between 5K to 300K. The coercivities obtained from the MH curves are then plotted against temperature (T). The magnetization in the films does not saturate, even at the highest field of 7T. The high field part of the M Vs H curves is fitted using the H1/2 term of Chikazumi expression M(H)= Q*(1- a /Hn), with n=1/2. The variation of coefficient 'a' of H1/2 term has been observed with temperature (T). An attempt has been made to correlate this with the coercivity (Hc) in the case of annealed films.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。