油酸和十二烷酸包覆的Fe3O4纳米粒子的磁性
Magnetic properties of Fe3O4 nanoparticles coated with oleic and dodecanoic acids
摘要:
合成了油酸(OA)和十二烷酸(DA)包覆的Fe 3 O 4磁性纳米粒子(NP),并通过透射电镜(TEM)、磁化强度M和交流磁化率测量对其进行了研究。OA涂覆的样品用不同的磁性浓度(78、76和65%)生产,DA样品用63%的Fe 3 O 4生产。来自TEM的图像表明NP具有近球形几何形状和平均直径约5.5nm。在不同的外部磁场H下,在零场冷却(ZFC)和场冷却(FC)工艺中进行的磁化测量在ZFC曲线中的给定温度TB处表现出最大值,其取决于NP涂层(OA或DA)、磁铁矿浓度和H。温度TB随着H的增加而单调降低,并且对于给定的H,磁铁矿浓度的增加导致TB的增加。所观察到的行为与NP之间的偶极相互作用(DI)有关,这似乎是所有研究样品中的一个重要机制。这一点得到了交流磁化率Xac测量结果的支持,其中不同频率的X'峰值温度遵循Vogel-Fulcher模型,这是偶极相互作用系统中常见的特征。具有不同涂层和磁铁矿浓度的样品的H与TB/TB(H=0)的曲线塌陷成通用曲线,表明样品的定性磁性行为可以由NP本身描述,而不是涂层或偶极相互作用的强度。在TB以下,M与H的曲线示出了随着温度降低而单调增加的矫顽场(HC)。饱和磁化强度(MS)遵循布洛赫定律和MS值在室温下高达78 emu/g的估计,结果对应于约80%的体值。给定样品的M/MS与H/T曲线的重叠和高温下的低HC表明研究的所有样品中存在超顺磁性行为。不同样品在恒定温度下的M/MS与H曲线的重叠表明NP磁化行为被保留,与涂层和磁铁矿浓度无关。
英文摘要:
Magnetic nanoparticles (NP) of magnetite (Fe3O4) coated with oleic acid (OA) and dodecanoic acid (DA) were synthesized and investigated through Transmission Electron Microscopy (TEM),magnetization M, and ac magnetic susceptibility measurements. The OA coated samples were produced with different magnetic concentrations (78, 76, and 65%) and the DA sample with 63% of Fe3O4. Images from TEM indicate that the NP have a nearly spherical geometry and mean diameter ~ 5.5 nm. Magnetization measurements, performed in zero field cooled (ZFC) and field cooled (FC) processes under different external magnetic fields H, exhibited a maximum at a given temperature TB in the ZFC curves, which depends on the NP coating (OA or DA), magnetite concentration, and H. The temperature TB decreases monotonically with increasing H and, for a given H, the increase in the magnetite concentration results in an increase of TB. The observed behavior is related to the dipolar interaction (DI) between NP which seems to be an important mechanism in all samples studied. This is supported by the results of the ac magnetic susceptibility Xac measurements, where the temperature in which X' peaks for different frequencies follows the Vogel-Fulcher model, a feature commonly found in systems with dipolar interactions. Curves of H vs. TB/TB(H=0) for samples with different coatings and magnetite concentrations collapse into a universal curve, indicating that the qualitative magnetic behavior of the samples may be described by the NP themselves, instead of the coating or the strength of the dipolar interaction. Below TB, M vs. H curves show a coercive field (HC) that increases monotonically with decreasing temperature. The saturation magnetization (MS) follows the Bloch's law and values of MS at room temperature as high as 78 emu/g were estimated, a result corresponding to ~80% of the bulk value. The overlap of M/MS vs. H/T curves for a given sample and the low HC at high temperatures suggest superparamagnetic behavior in all samples studied. The overlap of M/MS vs. H curves at constant temperature for different samples indicates that the NP magnetization behavior is preserved, independently of the coating and magnetite concentration.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。