基于掺杂有Er3+的非晶硅低价氧化物的谐振结构,具有硅纳米团簇,用于在1550 nm处的有效发射
Resonant structures based on amorphous silicon sub-oxide doped with Er3+ with silicon nanoclusters for an efficient emission at 1550 nm
摘要:
我们提出了一种共振的方法来提高1550 nm的发射效率的非晶硅低氧化物掺杂Er 3+(a-SiOx)层与硅纳米团簇(Si-NC)。<Er>两种不同的技术相结合,以提供一种结构,允许增加约12倍的1550 nm的发射。首先,通过常规的湿氧化获得SiO2层,并通过反应性RF共溅射沉积a-SiOx基质。<Er>其次,由于在相同的a-SiOx基质上通过在1150 ℃下的硬退火形成Si-NC,产生了Er 3+的额外泵浦沟道(4I15/2至4I9/2)。<Er>SiO2和a-SiOx厚度被设计为支持在泵浦波长(~500 nm)附近、在Si-NC发射(~800 nm)附近和在a-SiOx发射(~1550 nm)附近的谐振,从而增强光学泵浦过程。<Er><Er>
英文摘要:
We present a resonant approach to enhance 1550nm emission efficiency of amorphous silicon sub-oxide doped with Er3+ (a-SiOx<Er>) layers with silicon nanoclusters (Si-NC). Two distinct techniques were combined to provide a structure that allowed increasing approximately 12x the 1550nm emission. First, layers of SiO2 were obtained by conventional wet oxidation and a-SiOx<Er> matrix was deposited by reactive RF co-sputtering. Secondly, an extra pump channel (4I15/2 to 4I9/2) of Er3+ was created due to Si-NC formation on the same a-SiOx<Er> matrix via a hard annealing at 1150 C. The SiO2 and the a-SiOx<Er> thicknesses were designed to support resonances near the pumping wavelength (~500nm), near the Si-NC emission (~800nm) and near the a-SiOx<Er> emission (~1550nm) enhancing the optical pumping process.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。