银掺杂对La0(LBMO):Agx(x = 0.0,0.1,0.2,0.3,0.4)室温磁电阻的影响

Impact of silver addition on room temperature magneto-resistance in La0.7Ba0.3MnO3 (LBMO): Agx (x = 0.0, 0.1, 0.2, 0.3, 0.4)

Rahul Tripathi, V. P. S. Awana, H. Kishan, S. Balamurugan, G. L. Bhalla

摘要:

采用固相反应法合成了La0.7Ba0.3MnO3(LBMO):Agx(x = 0.0,0.1,0.2,0.3,0.4)复合材料,在1300 ℃(LBMO 1300 Ag)~ 1400 ℃(LBMO 1400 Ag)的烧结温度范围内,比较了它们的物理性能随温度和Ag含量的变化。所有样品均为单相结晶,随着银含量的增加,主结构相峰在高角度处发生一定程度的畸变。随着Ag含量的增加,晶格常数a,c减小,b略有增加。扫描电子显微镜(SEM)显示更好的晶粒形态的大小和扩散的晶界与Ag含量的增加。在LBMO 1300 Ag和LBMO 1400 Ag系列中,金属绝缘体转变(TMI)和伴随的顺磁-铁磁转变(TC)温度随着Ag含量的增加而降低。添加Ag的样品的MI转变,定义的电阻温度系数(TCR)的尖锐性,提高。在特定的Ag含量(0.3)下,TMI和TC被调谐到300 K,并且在该温度下实现了高达55%的最大磁阻(MR 7 T),这是在相同温度下对1300和1400 ℃系列的纯样品所观察到的磁阻的两倍以上。对于LBMOAg(0.4)样品,MR 7 T进一步增加到60%以上,但在270 K下。MR 7 T是在5、100、200、300和400 K的不同温度下在+/- 7特斯拉的不同磁场中测量的,其呈现U型和V型形状。总之,在LBMO中添加Ag显著改善了晶粒的形貌,并导致母体锰氧化物系统的更好的物理性能。

英文摘要:

La0.7Ba0.3MnO3 (LBMO):Agx (x = 0.0, 0.1, 0.2, 0.3, and 0.4) composites are synthesized by solid-state reaction route, the final sintering temperatures are varied from 1300 (LBMO1300Ag) to 1400 0C (LBMO1400Ag), and their physical properties are compared as a function of temperature and Ag content. All samples are crystallized in single phase accompanied by some distortion in main structural phase peaks at higher angles with increase in silver content. Though the lattice parameters (a, c) decrease, the b increases slightly with an increase in Ag content. The scanning electron micrographs (SEM) showed better grains morphology in terms of size and diffusion of grain boundaries with an increase in Ag content. In both LBMO1300Ag and LBMO1400Ag series the metal insulator transition (TMI) and accompanied paramagnetic-ferromagnetic transition (TC) temperatures are decreased with increase in Ag content. The sharpness of MI transition, defined by temperature coefficient of resistance (TCR), is improved for Ag added samples. At a particular content of Ag(0.3), the TMI and TC are tuned to 300K and maximum magneto-resistance at 7Tesla applied field (MR7T) of up to 55% is achieved at this temperature, which is more than double to that as observed for pure samples of the both 1300 and 1400 0C series at same temperature. The MR7T is further increased to above 60% for LBMOAg(0.4) samples, but is at 270K. The MR7T is measured at varying temperatures of 5, 100, 200, 300, and 400K in varying fields from +/- 7 Tesla, which exhibits U and V type shapes. Summarily, the addition of Ag in LBMO improves significantly the morphology of the grains and results in better physical properties of the parent manganite system.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑