Analysis of anisotropy crossover due to oxygen in Pt/Co/MOx trilayer
摘要:
对一系列Pt/Co/MOx(M=Al,Mg,Ta.)三层膜进行了特殊的霍尔效应和X射线光谱测量。为了研究氧化在Co/MOx界面处的垂直磁各向异性的开始中的作用。据观察,不同的氧化时间修改的Co层的磁性能,诱导从面内到面外的磁各向异性交叉。重点研究了等离子体氧化对Pt/Co/AlOx垂直磁各向异性的影响。通过X射线光电子能谱学测量分析了界面电子结构。它示出的面外磁各向异性的最大值对应于在Co/AlOx界面处的Co-O键合的显着密度的外观。
英文摘要:
Extraordinary Hall effect and X-ray spectroscopy measurements have been performed on a series of Pt/Co/MOx trilayers (M=Al, Mg, Ta...) in order to investigate the role of oxidation in the onset of perpendicular magnetic anisotropy at the Co/MOx interface. It is observed that varying the oxidation time modifies the magnetic properties of the Co layer, inducing a magnetic anisotropy crossover from in-plane to out-of-plane. We focused on the influence of plasma oxidation on Pt/Co/AlOx perpendicular magnetic anisotropy. The interfacial electronic structure is analyzed via X-ray photoelectron spectroscopy measurements. It is shown that the maximum of out-of-plane magnetic anisotropy corresponds to the appearance of a significant density of Co-O bondings at the Co/AlOx interface.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。